resumo

In this work glasses with nominal molar compositions 0.45SiO(2)-(0.45-x)MgO-xK(2)O-0.1(3CaO.P2O5) (x=0 and 0.09) were heat-treated according to adequate time-temperature schedules to obtain glass-ceramics (GCs) with phosphate phases. The GCs were immersed for different periods of time in SBF at 37degreesC. The morphology, crystallinity, and adhesion of the apatite layers thus formed are compared and discussed for the glasses and the GCs. Adhesion measurements were performed for the GCs using the scratch test technique. Distinct adhesion behaviours of the newly formed apatite layers to the substrate were observed when the GCs composition is K-free or when it contains K. Adhesion parameters for the apatite coating on the K-containing GCs showed to be affected by the immersion time in SBF but were not time-dependent in the case of the K-free GCs.

palavras-chave

BIOCERAMICS

categoria

Engineering; Materials Science

autores

Queiroz, CM; Frade, JR; Fernandes, MHV

nossos autores

Partilhe este projeto

Publicações similares

Usamos cookies para atividades de marketing e para lhe oferecer uma melhor experiência de navegação. Ao clicar em “Aceitar Cookies” você concorda com nossa política de cookies. Leia sobre como usamos cookies clicando em "Política de Privacidade e Cookies".