Electrophoretic deposition has been successfully used for the preparation of multilayer composite thick films of the temperature stable microwave dielectric ceramics BaLa4Ti4O15 (BLT) (epsilon(r) = 44, Qf(0) = 44,000 GHz) and Ba4Nd9.33Ti18O54 (BNT) (epsilon(r) = 82, Qf(0) = 10,000 GHz). The composites exhibit permittivity intermediate between the end members that may be tuned by modifying the ratio between and/or thickness of each layer, thereby tailoring the films for specific applications. In demonstrating an alternative way to tailor functional properties, these results have broad implications for a large number of thick film-based devices. (C) 2012 Elsevier Ltd. All rights reserved.

palavras-chave

ELECTROPHORETIC DEPOSITION; BAO-LN(2)O(3)-TIO2 LN; CERAMICS; MICROSTRUCTURE; BALA4TI4O15; TECHNOLOGY

categoria

Materials Science

autores

Vilarinho, PM; Mahajan, A; Sterianou, I; Reaney, IM

nossos autores

Partilhe este projeto

Publicações similares

Usamos cookies para atividades de marketing e para lhe oferecer uma melhor experiência de navegação. Ao clicar em “Aceitar Cookies” você concorda com nossa política de cookies. Leia sobre como usamos cookies clicando em "Política de Privacidade e Cookies".