HFCVD diamond deposition parameters optimized by a Taguchi Matrix

resumo

A Taguchi Matrix was used for the experimental design to study the CVD diamond deposition parameters in a cold-wall HFCVD reactor. Gas composition, total gas pressure, total mass flow and substrate temperature were considered as controllable factors, and three levels for each of these factors were selected, in an L9 orthogonal array. A new Figure-of-Merit (FOM) is proposed to assess the best combination of film properties: grain size, residual stress, structural quality and growth rate. Substrate temperature affects mostly grain size and diamond quality, while methane content mostly determines residual stresses and the growth rate. The latter is also mainly affected by the total pressure as well as is grain size, while total gas flow has a neutral effect. Under the limits of deposition conditions, the best FOM is obtained at the highest total gas pressure and mass flow, average CH4 content, and lowest substrate temperature. (C) 2010 Elsevier Ltd. All rights reserved.

palavras-chave

HOT-FILAMENT CVD; FILMS; SYSTEM; PRESSURE; QUALITY; GROWTH

categoria

Materials Science; Physics

autores

Salgueiredo, E; Amaral, M; Neto, MA; Fernandes, AJS; Oliveira, FJ; Silva, RF

nossos autores

agradecimentos

E. Salgueiredo, M. Amaral and M.A. Neto acknowledge FCT for the grants SFRH/BD/41757/2007, SFRH/BPD/26787/2006 and SFRH/BPD/45610/2008, respectively.

Partilhe este projeto

Publicações similares

Usamos cookies para atividades de marketing e para lhe oferecer uma melhor experiência de navegação. Ao clicar em “Aceitar Cookies” você concorda com nossa política de cookies. Leia sobre como usamos cookies clicando em "Política de Privacidade e Cookies".